Re: [MW:35280] parent mental is 25crmo4 to 25crmo4. Is 80S-B2 filler material is suitable or anything else one plz suggest
90S-B3 is overmatched. B3 weld chemistry is 2.25Cr + 1Mo
Not necessary. 80S-B2 is more than enough.
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE, CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015, ISO 3834, EN 15085,
International Welding Engineer.
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349
On Tue, Sep 17, 2024 at 10:01 PM vignesh musical <vikkismithsmith@gmail.com> wrote:
Dear1. TIG/MIG Welding:ER80S-B2: A filler wire designed for welding Cr-Mo steels. It has good creep resistance and is suitable for high-temperature applications.ER90S-B3: This wire provides higher strength and creep resistance than ER80S-B2 and is appropriate for critical applications where higher tensile strength is needed.--On Tue, Sep 17, 2024, 9:33 PM Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:25CrMo4 is equivalent 0.25%C, 1%Cr, 0.25% Mo which almost matches ur rod selection 80S-B2THANKS & BEST REGARDS,KG.PANDITHAN, BE, IWE, CSWIP 3.1,ISO 9712 Level 2 in VT,ASNT-Level II in PT,MT,RT & UT,LA ISO 9001-2015, ISO 3834, EN 15085,International Welding Engineer.CONSULTANT-WELDING & QUALITYMobile no: +919940739349--On Sun, Sep 15, 2024 at 3:34 PM Mehul Patel <vmgmehul@gmail.com> wrote:Dear Experts'Plz suggest me filler metal for 25crmo4 & explain 80S-B2.--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/168bfb14-9d86-4c3a-84d5-45ad0c8f4224n%40googlegroups.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNQh5u%3D_aCeXmhAoctO0ODV6OBNCP3EnSh7inJ6Hyc8sA%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFm2zHvt9okrddnVfR9h8q_%2BXTyMFt%3Dx92t8EAOcC11nui7nOw%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eN75Z-StbDGK6%2B7SSJnKSsmaN5A1JW2M_ZhYTqyWZDwzg%40mail.gmail.com.
Comments