Hello Experts,

Scenario
We have a weld joint where 10 mm thick SS pipe (P 8) is welded to 40 mm thick CS (P 1) flat cover. It is a partial penetration weld with 10 mm groove depth. The construction code is ASME Sec VIII Div. 1 and MDMT is -40 degree celcius. I am willing to use ER 309 LMo. 

Query
1. Do i have to use WPS with impact at or colder than -40 degree celcius, or only impact tested filler is enough? or, 
-YES

2. PQR without impact test will do if i am using non impact tested filler?
-NO.

Regards,
Pravin Katkar

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d06e2414-1c71-4660-81a6-2e4a4237823fn%40googlegroups.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...