Hai Experts,
Greetings!!

Hope you are doing well.
We found crack on Turbine Exhaust Stack butt weld joints made by 6 mm thick, SA 387 Grade 22 Cl.2 

We repaired with E91T1-B3 with FCAW welding process  with a preheat of 140 degree C , maximum Interpass temp. of 240 degree C.
But again welding crack observed while doing the MPI, request to please share your comments to solve this matter.


Thank You & Regards
Williams P Wilson
+968-94600828
QA/QC Engineer
Please consider the environment before printing this message

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHBxnQ58SLoK7ZkMmOVKrnTqCxCKrgQ%3DMNYWPZi8ZeBH-%2B5yNw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...