Re: [MW:35263] SA335 P91 to SA106Gr.B Dissimilar Material Welding Procedure

Dear Vijay Kumar,

Please refer API RP 582 , Table A.1

Thanks & Regards,

 

Raviraj Gohil | Manager - Welding | + 83473 02025 | www.lloydsengg.in 




On Mon, Sep 16, 2024 at 1:07 PM Vijay Kumar <vijaytuty@gmail.com> wrote:
Dear Experts,

I need SA335 P91 to SA106Gr.B Dissimilar Material Welding Procedure with some reference codes. 

Please share 

Thanks 
Vijayakumar
+91 8238450968

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/be7e26e6-2446-4b69-8ed4-d10c5a074dcfn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BN2U4Pgwb1euygiei628vD0m2PK1dVpu4hXEdXa0ZoNp-coEQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...