Re: [MW:35238] Overlay welding defects

To prevent defects such as pinholes and blow holes in welding overlay, especially in overlapping joints, consider the following approaches:

1. Pre-Welding Preparation

- Material Cleanliness: Ensure that both overlay and base materials are clean and free from contaminants like oil, grease, and rust.
- Edge Preparation: Properly prepare the edges to be welded, ensuring appropriate fit-up to minimize gaps.

2. Welding Parameters

- Heat Input Control: Adjust the heat input to avoid overheating, which can lead to excessive dilution and defects.
- Travel Speed: Optimize travel speed to ensure adequate fusion without excessive heat.
- Electrode Type: Use suitable electrodes or filler materials that match the base and overlay material properties.

3. Shielding Gas

- Gas Composition: Use appropriate shielding gas to protect the molten weld pool from contamination.
- Flow Rate: Ensure proper gas flow rates to avoid turbulence that can trap gas in the weld pool.

4. Post-Weld Treatment

- Heat Treatment: Consider post-weld heat treatment to relieve residual stresses and improve mechanical properties.
- Inspection: Conduct thorough inspection (e.g., NDT methods) after welding to identify and address any defects early.

5. Welding Technique

- Weaving Pattern: Utilize appropriate weaving techniques to ensure uniform deposition and minimize defects.
- Control of Interpass Temperature: Monitor interpass temperatures to prevent overheating and promote proper solidification.

6. Environmental Factors

- Welding Environment: Perform welding in controlled conditions to minimize the effects of moisture and contaminants.
- Drafts and Wind: Protect the welding area from drafts and wind that could affect the shielding gas coverage.

7. Training and Skill Development

- Welder Training: Ensure that welders are trained in techniques specific to the materials being used, especially for high-performance alloys like Inconel.

By following these guidelines, you can significantly reduce the occurrence of defects in welding overlays. Regular monitoring and adjustments based on specific conditions will also help in achieving better outcomes.

On Wed, Sep 4, 2024 at 2:58 PM Karthick Flow Controls <kfccovaigm@gmail.com> wrote:
Dear Experts,

Welding Overlay, After Machining the Pin holes and blow holes noticed in Overlapping Joint area, After attend the defects, It will open some other places, The defects noticed Uniform inline.   ( Overlay Material ,316L ,Inconel 625 ,St6 & ST21,Base Material WCB/LCB),
How to prevent the defects?




Regards,
R.Gowtham.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/33a4e532-e9d1-45f0-a35f-2172b2263b12n%40googlegroups.com.

The information contained in this email is intended for use only by the recipient to whom or which this is addressed. Such information may be privileged, confidential, and/or proprietary subject to the GMEC Email Disclaimer. Moreover, as we value your privacy, we will handle and safeguard any personal data we receive in this email in accordance with our Privacy Notice.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFizHVXX8FYkaDWwAx8e%2Bbo9ckbOJ4hQZd3cpmNJ%2B5bH97ptxw%40mail.gmail.com.