Re: [MW:35194] Re: WELD DISTANCE AS PER ASME

Reference code like ASME Sec IX never say on this matter. It is given in Referring code like Sec 8, 1
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Tue, Aug 27, 2024 at 3:17 PM S P Ali <syabuzar@gmail.com> wrote:
ASME does not outline this, whereas some British standards, such as "BS 4515:2009," require 4 times the wall thickness of the thinner part to be joined.

ARAMCO says in "SAES W11" spacing shall be 3x wall thickness or 20mm, whichever is greater.

If you're working on a project, double-check the specifications or applicable code. If you're preparing for an interview, remember both.

On Tuesday, May 2, 2017 at 9:46:40 AM UTC+3 hajarath ali wrote:
Not required any minimum distance between Socket weld joint as per ASME B31.3.

Referance : 

B31.3 Interpretations No. 14 Interpretation: 

Question (4): Does ASME B31.3-1993 Edition, Addenda b, have requirements for the minimum lengths of pipe sections between welds? 
Reply (4): No


On Sunday, April 23, 2017 at 9:01:07 AM UTC+3, Faizal, Majeed [c] wrote:

Can anyone please confirm the Minimum distance between Socket weld joint as per ASME B31.3 where its specified.

 

Regards,

 

Faizal

 

 

 

 

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1f085422-cb32-4ede-9502-86b7808aad78n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNaYXwXHtd63gUcT_jOuRi1j9UABbZx6m3Q5Ki_cVqF5g%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...