Dear,

Thank you for your reply. My doubt is which section we need to refer ISO 15614-1 for steel or ISO 15614-2 for Aluminium. Aluzinc is coating on steel sheet.

Thanks & Regards
Ganesh

On Sat, 24 Aug 2024, 7:24 am Raviraj Gohil, <raviraj.gohil@lloyds.in> wrote:
You may use ISO 15614 for Procedure qualification and ISO 9606 for welder qualification.

Thanks & Regards,

 

Raviraj Gohil | Manager - Welding | + 83473 02025 | www.lloydsengg.in 




On Thu, Aug 22, 2024 at 3:40 PM Ganesh R nair <ganeshrnair9@gmail.com> wrote:
Dears,

Which ISO standard shall be followed for qualification of WPS and Welders on Alu Zinc material (2mm).

Thanks and regards,
Ganesh R Nair

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJ_8oJUHeMm2pPD9aVB0qSk3b3Gi%3DrFw4zvPwYG5kdpOGs3CPw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BN2U4MygX44tZHXOxcvDMNPDdMxr0DEUrhAan1cg5p0Jcr-vA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJ_8oJX8g9bcv39%2BBhL0tn6eHo7jC6rUTDWbwppVWfGsW7ZBMA%40mail.gmail.com.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...