Dear Biju,

It's unlisted to unlisted material qualification, specific material grade.

Change in material grade requires new qualification as per AWS D1.1

Regards
Shahil 

On Sun, Aug 25, 2024, 16:36 Biju H <biju.psl@gmail.com> wrote:
Dear Sirs,
if we are qualifying a PQR with EN10025 S355JR to S355JR is this PQR qualifies to weld S355J2 to S355J2?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADWuZ7XiuQGFqh3Mof6QavNjiOVmGUQ5a_ZvEm6-kc0Xbt9itQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALfBO__odY2ZXz1OG_muUh4kYkzhhaRjoqKBp2SG3zXfQm9XdQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...