Saturday, August 24, 2024

Re: [MW:35176] Filler wire for 321H

Hi,

You can use 321 with higher carbon content .

You need to ensure carbon content of filler wire .


On Fri, 23 Aug, 2024, 8:07 am Vignesh Manoharan, <vkemano@gmail.com> wrote:
Hi experts, 

What filler wire is required to weld 321H in GTAW process. ? 

Pls suggest


Regards
Vignesh M

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOUncPL9Nh0PigpmvCq8YDrd%2B2SQsikfyt6_q0_ZU2RZ-aC7jg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADXbd_dCYr0zQ%3Dq2W8gbAvL9TUOx%3DG%3DJdaeEXofDbsYbENW%2BvA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...