Re: [MW:35175] Filler wire for 321H

If GTAW, use 321 H if it is available otherwise 321 itself. IF process other than GTAW, use 347 
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Fri, Aug 23, 2024 at 8:07 AM Vignesh Manoharan <vkemano@gmail.com> wrote:
Hi experts, 

What filler wire is required to weld 321H in GTAW process. ? 

Pls suggest


Regards
Vignesh M

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOUncPL9Nh0PigpmvCq8YDrd%2B2SQsikfyt6_q0_ZU2RZ-aC7jg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNi9Z2AvGqddBPSTRjVXiBy2HjFrwO7h1pPz_7pnvih2A%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...