Re: [MW:35152] Re: RELATED WPS AND FILLER WIRE

Please give me ASME reference. Where it's mentioned


On Thu, 1 Aug 2024, 3:05 pm Shivasankar A, <shivasankar2593@gmail.com> wrote:
HI Vishal,

If your WPS qualified in the sequence of process GTAW+SMAW, and deposited weld thickness of GTAW is minimum 3.5mm. then you can proceed with full GTAW with ER 70S-2 Filler Wire.

regards,
A.Shivasankar

On Monday, July 29, 2024 at 3:16:48 PM UTC+5:30 Vishal Kumar wrote:
Hii Expert,

I have WPS SMAW + GTAW (5.5  MM THK.-DEPOSITED 11 MM THK)-MATERIAL ASTM 106 GRB , CAN USE SAME WPS IN FULL GTAW WELDING METAL THK. IS 7 MM..


And I have C-1020 material which filler wire & Electrode  can use in full GTAW PROCESS and SMAW PROCESS


THANKS

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bed83631-80c1-4aea-87c3-983490d499acn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEabyK%3Dy%3D%2BOybqVYgMVpggKx4O%2B4%3Dez4YqhQFc7w%2BN65Pvohkw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...