Re: [MW:35041] Heat treatment

NACE MR 0175 refers only to the hardness value, not PWHT. Its requirement of client/ designer

On Tue, May 7, 2024 at 3:20 PM Shahil Saini <sainishahil98@gmail.com> wrote:
Dear all,

Can we Exempt PWHT of Weld metal as per NACE MR0175/ISO 15156-2 for carbon steel? Is there any metallurgical changes that will affect the material??

Regards,
Shahil Saini 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALfBO_8MvjYQsKmSSrVWC3erO3YeWxCDTaNrWZQKRGhEbu6WXQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8kwNbtip5mAMSD9tSnqfuE2rtNEw1xkgDWgov1GHu6Biw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...