Dear experts,

Is it required UT or RT for annular plate butt weld joint in less than 10mm plate 
Our annular plate thickness is 6MM.

I have some confusion from the standard 
Below I attached Standard 




Thanks & Regards

Navaneetha Perumal S

QA/QC Supervisor -Mechanical & Welding

CSWIP 3.1, NDT Level-II & ISO 9001:2015

:+966-505721787 (WhatsApp & Calling)            M :+919750521128

ThinkGreen before printing this email.

10 Liters of water is required to produce one sheet of A4 paper

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOj8udMORQQAG-FDZ8-K846Esw9iZu3MhvhLOU-LrnN4WLwnfw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...