Re: [MW:34960] PQR AWS D1.1

Dear,

Certainly, according to AWS D1.1, the qualification of Procedure Qualification Record (PQR) for pipes is indeed possible. The relevant clause in AWS D1.1 that addresses this is typically Clause 3, "Qualification." This clause outlines the requirements and procedures for qualifying welding procedures, including those for pipes.

To qualify a PQR for pipe welding under AWS D1.1, you would need to follow the guidelines outlined in Clause 3, which includes considerations for thickness, diameter, and testing requirements.

Here's a summary of what AWS D1.1 typically requires for qualifying pipe PQRs:

  1. Thickness Range: Specify the range of pipe thicknesses for which you intend to qualify the procedure. AWS D1.1 usually provides guidelines for the minimum and maximum thicknesses that can be included in the qualification.

  2. Diameter Range: Similar to thickness, specify the range of pipe diameters for which you intend to qualify the procedure. This may vary based on project requirements and industry standards.

  3. Testing Requirements: AWS D1.1 typically specifies the testing requirements for qualifying welding procedures. This may include various non-destructive testing (NDT) methods such as ultrasonic testing (UT), radiographic testing (RT), magnetic particle testing (MT), or dye penetrant testing (PT), depending on the specific welding process and material.

To provide specific qualification ranges for thickness, diameter, and testing, it's important to refer directly to the AWS D1.1 code for the most up-to-date and accurate information. Additionally, consulting with a qualified welding engineer or inspector can help ensure that the qualification process aligns with the requirements of AWS D1.1 and any other applicable codes and standards.

Regards,

AB


On Tue, 7 May 2024 at 14:14, saleem manhappulath <saleemm9526@gmail.com> wrote:
Dear All

   I have situation, kindly advise the solution 

Can we qualify PQR in pipe in AWS. D1.1. If we can please suggest qualification range . Thickness , dia and testing 

Thanks & Best Regards
Saleem manhappulath

Mob:+966533595849
WhatsApp:+919526445936

From iPhone xs

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKH3Oms3iAKJnAg2Am7Ysx7RswowxX5zAPaiAnkrgEFZ8X7_Fw%40mail.gmail.com.


--
Best regards,

Amol K.B
B.E(Mech), CSWIP 3.2.2, NACE CIP 1 & ASNT LII(4M)

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAADcG1qbc5gLqqvX4%3Do0WmXPenKSJ4y-QG92%2BFUBc-9s6vb2hQ%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...