Dear Experts,

1.Can anyone tell me what is meant by Cold pass in Dss/Sdss welding. Also please tell me the difference between Hotpass and Cold pass.

2.In DSS Pipeline welding Root pass is being performed with SDSS consumable and rest is performed with DSS consumable.  Can anyone explain me why it is performed like this

Thank you 