Re: [MW:35034] Interpass Temp. Max

You can consider it 315º C as per API RP-582 considering ASME Sec. IX P-No. 1 material.

Thanks 


C. R. GANDHI

On Wednesday, May 29, 2024 at 10:14:20 AM GMT+5:30, P NAVEEN <pnaveen010@gmail.com> wrote:


Hii,

What will be max Interpass temp of E 250 Br material in SMAW process.


Thanks

--