On Sat, May 11, 2024 at 8:52 AM KATHIRAVAN MURUGESAN <kathiravanmurugesan07@gmail.com> wrote:
Hi all 

Can u explain anyone where it will be mentioned in take welds must be weld in qualified welder's.

Sex ix or b31.3

On Tue, May 7, 2024, 7:35 PM saleem manhappulath <saleemm9526@gmail.com> wrote:
Dear All


    I have a ss wps P-8 to P8, i have plan to qualify welder. Can I use cs material for welder qualification with ss wps

Thanks & Best Regards
Saleem manhappulath

Mob:+966533595849
WhatsApp:+919526445936

From iPhone xs

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKH3OmvOBHxLj-_j4XRJQ-WwN6--u79GGcQr_zND%3DQE4ye%2B6QA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADsXJ%2BMU-bq3EViqRsX%3DU-wbYVSJByi7njmL_ow7Fjn_WoiG0g%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGJf7So1BOdQ5xyG7fm%2BS6D9DfeKk2441-SvHC118eEpFR9vfQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...