Re: [MW:34772] P-No. of UNS 06626

Dear Fauzi,

Please refer to the Limiting chemical composition in MTC & concerning ASME Code Case 2276 
It should be P-No. 43



On Wed, Feb 28, 2024 at 11:12 AM ilham fauzi <ifilham@gmail.com> wrote:
Dear Experts,

What is P-No. of UNS 06626, my client say its P No.45 but that materials simillar with UNS 06625 which is its P-No.43. Please for the advice

Thanks

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c105a43f-72c7-44b6-96e1-0e11095552a3n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN4%2Bm0zqEw6VA8bxt9wrr882YY8HAa2kWS_Zbd0cEfNMq%3DMr%3Dg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...