Tuesday, February 27, 2024

Re: [MW:34767] PQR for Piping - NDT Acceptance criteria

HI
you can refer only to ASME Sec IX for PQR because B31.3 also gives directions, But  NDT for piping welds you want to refer to B31.3 based on Category D,or M ... .

On Tue, Feb 27, 2024 at 3:13 PM 'SENTHILKUMAR SWAMINATHAN' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Hello Dears,

Please give you input when PQR for Piping done - Client spec is silent in NDT Acceptance criteria. Which code Acceptance criteria should use for NDT?

ASME B31.3 or ASME IX.

Thank you, 
Regards, 
S.SENTHILKUMAR

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/750277828.828737.1709031941988%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEE6DzffbS6xKHz%3DUMq1idrQPVg7zYDpxbo%3DQu0F1okgDE6PRQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...