[MW:34755] Re: Welding requirements of Centralloy G4852Micro and ET45 Micro


On Thursday, February 15, 2024 at 10:59:21 AM UTC+3 maheshQAQC wrote:
Dear Experts,

Need your Kind Inputs of welding requirements of Centralloy G4852Micro and ET45 Micro, we have upcoming project which we required to Qualify procedures.

and kindly share a sample WPS/PQR and fabrication procedure if you have any.

your Valuable inputs are highly appreciated and thank you.

regards.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0480dd00-2683-4ced-a28d-ce337a7404d1n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...