Dear sir.
Please share with me the Proposed welding procedure procedure. Which can help me make PQR.
On Mon, Feb 26, 2024, 1:34 PM Antonio Magalhães <8371935julio@gmail.com> wrote:
Dear,I have all the info for welding requirements this material (Furnace)--A sexta-feira, 23 de fevereiro de 2024 Ã (s) 08:11:54 UTC, Mohd Siraj escreveu:
- Centralloy® G 4852 Micro datasheet: https://www.schmidt-clemens.com/fileadmin/sc-downloads/werkstoffdatenblaetter/WST_4852_Micro_161109.pdf
- Centralloy® ET 45 Micro datasheet: https://www.schmidt-clemens.de/fileadmin/sc-downloads/werkstoffdatenblaetter/WST_ET_45_micro_161109.pdf
On Thursday, February 15, 2024 at 10:59:21 AM UTC+3 maheshQAQC wrote:Dear Experts,Need your Kind Inputs of welding requirements of Centralloy G4852Micro and ET45 Micro, we have upcoming project which we required to Qualify procedures.and kindly share a sample WPS/PQR and fabrication procedure if you have any.your Valuable inputs are highly appreciated and thank you.regards.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2051f87e-5612-4b37-befd-61d48971ace3n%40googlegroups.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGui1QmSyYgkacR2O_UqoktK%2BND7dMW%2BPvjsYiS%2BQDbe7YXQ0A%40mail.gmail.com.
Comments