What is diameter of the sphere?
Sent from my iPhone

On 09-Feb-2024, at 6:29 PM, Amit Hotkar <amithotkar1987@gmail.com> wrote:

Hello, 

We are in bidding stage of sphere in 121mm THk Material A 516 Gr.70N HIC and code of construction ASME dev VIII Div-2 , coded.

Can you please guide us  below question 

1.Do we able to use alternate method from SMAW for HIC plates? if SAW or other which welding machine with theoretical productivity, performance details & price details of welding machine ? 

2. Type of Arrangement details to hold welding machines on vertical seam & circumference seam.

3.Butt weld details like type groove, groove thickness, sketch for groove dimensions with number of weld layers / pass.

Regards
Amit 


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/fbe6aea7-be80-4d99-b126-90bbdd2a6599n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...