Re: [MW:34754] Aluminium plate material testing

Dear All :
Hitherto we were using EWTh-2 confirming to AWS SFA 5.12 . We are now advised by consultant to opt for EWLa-2 i.e .2 % lanthanated Tungsten electrodes .. Any experience by experts and which standard it qua

On Tue, 30 Jan 2024 at 12:29, md.az...@gmail.com <md.azhar23@gmail.com> wrote:
Hii , can you please tell me about aluminum raw materials (Plate) sampling which BSEN std is applicable.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/12342641-2464-41c7-bf67-ec8f027bd565n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BQ29OgkEf%3DwO0%3D8ZvXcW3PzrQEEguuN3rQ9cEtbNK1kg6KFGA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...