GTAW weld metal depoisted thickness 3.5 to 4mm

On Mon, 22 May 2023, 07:44 Jenish Mistry, <jenishmistry1992@gmail.com> wrote:
Dear sir ,

Please confirm the weld Deposit thickness for the GTAW process...

On Mon, May 22, 2023 at 8:40 AM Prasad rao <prasadrao31@gmail.com> wrote:

Dear All,


We have prequalified WPS of combination  GTAW+SMAW

 

Qualified material :4"  Dai X Sch-120(11.02mm)

Garde : ASTM A106 GR B

Welding Process :  GTAW +SMAW


Construction Code : ASME SEC IX

 

Root/ Hot : ER70S-6 Dai 2.4

Fill 1,2 ,3 : E7018 Dai 3.2

Cap           : E7018 Dai 2.5.

 

With Above WPS I would like to extract new WPS for GTAW Process. Please Kindly confirm  what shall be the range  for GTAW process  for parent material thickness . Kindly advice. with reasoning.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEML-XTU9igHwEckWNCH4r_XuWwozo4qRoC_yEXuMvkQrpSuEg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADXbd_fUXMTYF1Ezem7Q_zgt_Rk%3Dmh4R9VwGr9SL7vdH0Mfskw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEML-XSFx8z-iZGPBN%2B_XuyT%2BkiLwrOO2%2Bi5%3Dp5MUYeaLg%3DyLQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...