[MW:34246] RE: 34244] Max allowable machining thickness for qualifying PQR

No problem sir, the range qualify will be base on the actual thickness of test coupon/

 

From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> On Behalf Of JITHIN GOPINATH
Sent: Sunday, May 28, 2023 1:54 PM
To: materials-welding@googlegroups.com
Subject: [MW:34244] Max allowable machining thickness for qualifying PQR

 

Sir,

Can anyone advice me about the maximum allowable machining thickness for qualifying PQR.

For example I have a pipe with thickness 15.88 I want to reduce the thickness to 12.6 is that possible? If there any limitations for machining the thickness..

Please advise...

 

Regards

Jithin

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAT3KQ7iuBvsLQTWYfFSvHRunVEd%2B_jHsd_vEZMVKozOt%2BKcfw%40mail.gmail.com.


Virus-free.www.avast.com

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...