[MW:34234] Re: PQR Qualification _welding electrode

Rajesh

No further qualification is required. Refer AWS A 5.36, it is mentioned there. This is relatively a new standard published by AWS.

On Thursday, October 4, 2018 at 5:14:43 AM UTC+3 RAJESH KUMAR wrote:
Dear Team,

For our PQR qualification ( Done in 2018) to flux coared wire for carbon steel,we use the wire clasified SFA/AWS A5.20  E71T-1C/1M/9C9M.

Today we received from our supplier wire classified SFA A5.36 E 71 T-1C 1A2-CS1.

The classification is different,so we have to issue new PQR qualification required?



Thanks & Regards

Rajesh kumar
055-5251449
Sharjah

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/fa190138-86d9-483e-ae28-2a3cf1709671n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...