Only Chemical Analysis
Thanks & Regards
J.Gerald Jayakumar
On Wednesday, 17 May, 2023 at 01:44:58 pm IST, sujit kumar <sujitkumar19942@gmail.com> wrote:
Dear
Vishwas Keska
SFA NO-5.9
AWS NO-ER316L, ER347,ER308L,
SFA NO-5.14
AWS NO-ERNICr-3
Please find the above sfa no and aws no for your reference.please explain what test require as per asme section II part C.
Thanks & Regards
Sujit
On Wed, 17 May 2023 at 13:04, Vishwas Keskar Welding Manager WELDING <vvkeskar123@gmail.com> wrote:
Which specification and AWS wire ?Pl refer respective specification/AWS name for required tests in ASME SEC II CThe consumable mfg er will issue certificate as per that specification .If you need particular batch to be tested and need results which was shipped to you , this requirement shall be addressed in Consumable PO thr TDCThanksVishwas -IWE--On Wednesday, May 17, 2023 at 11:55:00 AM UTC+5:30 sujit kumar wrote:Dear all,What Test is required for filler wire as per ASME section II part C and what dimensions we have use for testing plate for filler.Best regards.SUJIT
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b1d21064-2722-4a64-a3c9-9793bbcfa3b7n%40googlegroups.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFonYWPbs91njze9QRF0R2S7ewyRdmUCZFd2iqmTU3MiKDE%2Bnw%40mail.gmail.com.
Comments