Tuesday, May 2, 2023

[MW:34174] Re: IGC TEST FOR FILLER WIRE AND ELECTRODE.

Pl. ask Consumable supplier to issue CMTR . They will do testing and certify the batch with IGC Prac E 

Thanks 
Vishwas 
IWE 

On Saturday, April 29, 2023 at 1:17:10 PM UTC+5:30 sujit kumar wrote:
Dear all,

How to prepare the test piece for IGC Test for filler wire and electrode...? where is given the detail about test piece preparation detail....

IGC TEST procedure as per  ASTM A262 PRACTICE-E


Thanks and regards
Sujit

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1c6663ba-06ea-44e0-8564-5a01d877a783n%40googlegroups.com.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...