[MW:34253] RE: 34250] Re: Max allowable machining thickness for qualifying PQR

if you specify the design code, it will be easier to respond to your inquiry. However, according to ASME B31.3 you can Taper the wall thickness maximum to 30 degree.

 

 

 

 

 

 

From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> On Behalf Of biennd
Sent: Wednesday, May 31, 2023 12:17 PM
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:34250] Re: Max allowable machining thickness for qualifying PQR

 

Taping to matching thickness --> ok.

 

On Monday, May 29, 2023 at 9:34:36 AM UTC+7 JITHIN GOPINATH wrote:

Sir,

Can anyone advice me about the maximum allowable machining thickness for qualifying PQR.

For example I have a pipe with thickness 15.88 I want to reduce the thickness to 12.6 is that possible? If there any limitations for machining the thickness..

Please advise...

 

Regards

Jithin

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b611ab5d-2901-4099-a3be-b9208e19d7a9n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...