Hi Zafar,
As per approved WPS you need to follow the same filler wire or electrode, You can switch for welders within the same F number and can use any filler wire.
For WPS strict to utilized as per Actual PQR.

Regards,

Muhammad Azeem Iqbal
Welding Inspector Aramco Approved
053110-8577/0554453626/0590071467




On Mon, 31 Oct 2022 at 06:12, Chaudhary Zafar Iqbal <chzaiqbal88@gmail.com> wrote:
Respected Member of this Group ,

As per approved wps ER70S-2 required to use .


Any code restrictions to use ER70S-6 instead of ER-70S-2 ?

Any code restriction and reference to change the WPS ?

Waiting for your valuable comments .

Regards,
Zafar 
00966544639978

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP9k9Xfz8xCCsA_t9CeOMw_Z506BBi5sX5wjT8SUuBrS9JrsZQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHqH7yCo0g6%3DZQJ82zq0zhu9fPU%3DLsgQcu0AFDbFdUvoo08_dg%40mail.gmail.com.

No comments:

[MW:35763] Hardness range for CS+ Alloy0625 clad welding

Dear experts. I am currently in the process of qualifying a PQR for API 5L X65 + A350 LF6. Both material consists of a base metal with alloy...