Dear Experts,

Could you please provide your additional comments on the attached test certificate of inconel Welding consumable.
ENiCrFe-3(SFA 5.11)

Also please share if anybody has the test certificate of the above electrode.

--
Thanks and Regards,
E. Anand,
Lead QA-QC,
Sohar,
Oman.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANOYChwZD9%3DbZ1021wnb5c9AWojoYU-mrQK%2BwvOpmNafNYNGSQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...