Saturday, November 12, 2022

Re: [MW:33697] HDPE Piping

Hi,
 Ot depends on your requirement and projects specs.
You may use: 

1. ASTM D3261
Or
2. AWWA as following (most used)

AWWA C 901-02, Standard for PE Pressure Pipe and Tubing, [13 through 76 mm] 0.5 in. through 3 in. for Water Service;
AWWA C 906-99, Standard for PE Pressure Pipe and Fittings, [102 through 1600 mm] 4-in. through 63 in. for Water Distribution and Transmission;

On Sat, 12 Nov 2022, 5:08 pm Anand Elankumaran, <email2uranand@gmail.com> wrote:
Dear Experts,

Could you please provide the standards for HDPE piping materials , Valves and flanges.

As far as I know, only ISO 4427-2 for pipes.

Could you please provide the remaining standards.


--
Thanks and Regards,
E. Anand,
Lead QA-QC,
Sohar,
Oman.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANOYChzsdiw6UOn2AEtLji5La_-nUBdJ7JXwTNnpM1zUu7dUGw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAE_Mq3OHyf1V5wOMJ2G3Wmfr1F%2B9qMLGiMLMXRU5dhTLY1m9QQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...