6010 doesn't required baking because it is being designed to have more ammount of Hydrogen around 60ml to give better penetration in cross country pipe. Hydrogen is being a non conductivity , it does not allow electric arc to flow smoothly, so more arc force is required to push the current which in tern gives deeper penetration.   IF U DO BAKING, HYDROGEN WILL GET VANISHED

On Wed, Nov 16, 2022, 8:52 AM Muhammad Azeem <azeem7999@gmail.com> wrote:
These electrodes are non low hydrogen electrodes which does not required baking before welding , Only need to keep in dry environment and used for downhill welding process. 

Regards,

Muhammad Azeem Iqbal
Welding Inspector Aramco Approved
053110-8577/0554453626/0590071467




On Tue, 15 Nov 2022 at 11:51, Bestun Ahmed <bestunahmed555@gmail.com> wrote:
Hi brother, 
No, no need to hold it or keep it in the oven.

Thanks

Bestoon


On Tue, Nov 15, 2022 at 8:26 AM Vishal Jaiswal <vis469jaiswal70@gmail.com> wrote:
Dear Sir,

               Please give information about ER 6010 electrode is need baking or holding in portable oven for the root welding of ERW pipes having thickness range 3 to 8 mm.
Please give suggestions.



Thanks and regards
Vishal kumar
Mechanical Engg.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF6t408Ks6qVdKS5qRuS06scPKDDzchmwsx01G20H3kb7Z71Tg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANd6T%2B_vDKQpAqGfCGt90zB_BW8jYs1%3Drs4Qx7gHiSyC24uxgQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHqH7yDQw7_MLGTgoE_DX4cXcNF%2Bh7W4_PVxSVbRC-8qMF3KNA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMvioF%2B2mVAJ%3DWBU-CEEvWRKoiZEWv5ULVD3dQ6%2BXKWjA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...