Tuesday, November 15, 2022

Re: [MW:33709]

Hi brother, 
No, no need to hold it or keep it in the oven.

Thanks

Bestoon


On Tue, Nov 15, 2022 at 8:26 AM Vishal Jaiswal <vis469jaiswal70@gmail.com> wrote:
Dear Sir,

               Please give information about ER 6010 electrode is need baking or holding in portable oven for the root welding of ERW pipes having thickness range 3 to 8 mm.
Please give suggestions.



Thanks and regards
Vishal kumar
Mechanical Engg.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF6t408Ks6qVdKS5qRuS06scPKDDzchmwsx01G20H3kb7Z71Tg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANd6T%2B_vDKQpAqGfCGt90zB_BW8jYs1%3Drs4Qx7gHiSyC24uxgQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...