Re: [MW:33783] Filler wire Button weld test

Hi sir,
Except Aramco standard. Can you explain from ASME codes 

On Tue, Nov 29, 2022, 7:05 PM Faisal Quadri <faisalquadri12@gmail.com> wrote:
SAES A 206  Aramco requirement 

On Tue, Nov 29, 2022, 1:25 PM Ponnikumar <k.ponni1994@gmail.com> wrote:
Dear gentlemen,
My client inspector told me to do button weld test on plate for filler wire 309L . The dimension are follow as asme sec II c then need to do PMI verification 

My query is any requirements by code for filler wire button test for all filler and electrode and why it required ? 



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKL%3DdYw73OyFYLq4yTHUB2cVqbuaDCCunxc73%2BaU0kJZurJd%2Bw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJwxg4e8MUi3dCWRoVTdphw1FNueJuUc8WcucN1nUtd58emFZw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKL%3DdYznh5WmCWEEx%3D8ReV0b4vHc-Bv0%3D6763kvuySqDNUztzw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...