Re: [MW:33102] Pig launcher

Please check with your GA (General Arrangement) drawing for Pig launcher what is the Code used or check your Design data sheet.

Thanks & Regards

J.Gerald Jayakumar




On Tuesday, 31 May, 2022, 11:26:12 am GMT+4, Benaouda Mezrar <mezrarbenaouda4@gmail.com> wrote:


can you please direct me in wich code i can find the acceptance criteria of NDT
For Example :
for piping acceptance criteria are in ASME B31.3 
for pipeline acceptance criteria are in API 1104 


Le mar. 31 mai 2022 à 06:35, 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> a écrit :
Pig launcher and Receiver design will be as per Pipeline Design code and the Closure will be as per ASME Sec.VIII Div.1 or 2.

Thanks & Regards

J.Gerald Jayakumar




On Tuesday, 31 May, 2022, 07:20:40 am GMT+4, Benaouda Mezrar <mezrarbenaouda4@gmail.com> wrote:


Dear experts kindly guide me

in which code i can find the acceptance criteria for the construction of pig launcher
and what is the desing code used (ASME B31.8 or ASME ASME-8)

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/9ac05358-95d4-40ca-b12d-51d014da78b9n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1093008174.2766849.1653970391846%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANKYR7sYS9Gd5rE491%2Bz0yhMCo6iknwAMfWJd1s%3DuGfdMnuJJA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...