Hi,
1. Inconel 625 to SS 304H : ENiCrFe-2 or ENiCrMo-3
2. Inconel 625 to SS316L : ENiCrFe-2 or ENiCrMo-3


Thanks& Regards,

(Karthik)
Karthikeyan.S
M: +66-892512282


On Monday, May 16, 2022, 12:05:37 PM GMT+7, chandra sekaran <chandrasekaran.vcs@gmail.com> wrote:


Dear experts kindly guide me For GTAW 

1. Inconel 625 to SS 304H : what filler wire can be use 

2. Inconel 625 to SS316L : 
What filler wire can be use

Regards

Chandrasekaran V

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN4ibzmvO7S7PhStVFoVfO%3D97tuRBY_f3_ak9Nz_hACR%3DEeTCw%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...