Hi
There is a tendency of Cracks in Fillet weld 
if
Set up is not proper I. e  uneven at matching /mating  surface causing distortion
There should be strong tack weld on both ends and on opposite sides
Improper st up causes heavy stresses on weld causes cracks
 Regards
Hegde


On Mon, 16 May 2022 at 8:43, 'kishore barbudhe' via Materials & Welding
<materials-welding@googlegroups.com> wrote:
Dear expert,

We observed transverse cracks after completion of fillet welding.
We are using EA2 filler wire in submerge arc welding and parent materials is E 450.
Please give us advice to resolve this issue.

Thanks & Regards

Kishore B 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1190457571.2472505.1652533602689%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/613859026.2720552.1652677328131%40mail.yahoo.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...