Re: [MW:33031] channels and bonnets with six or more tube passes

Please look into the attachment and advise that pwht is applicable for these channels as per API 660 clause 9.6.9 (a) or not?
Both channels are belongs to one HE.
Regards,
Manohar.

ClauseFrom: Raghuram Bathula <raghurambathula@gmail.com>
Sent: Tue, 05 Apr 2022 15:37:49
To: Materials-Welding <materials-welding@googlegroups.com>
Subject: Re: [MW:33030] channels and bonnets with six or more tube passes
 
it is from one end of HE to another end is consider as 1 pass (not individual channel)
 
On Tue, 5 Apr 2022 at 15:22, 'manohar matcha' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Dear Group Members,

Please share your opinion/interpretation on API 660 Clause 9.6.9 (a)


 
Tube passes to be considered for individual channel or both channels (if Exchanger is having 2 channels)?
 
in other words:
Individual Channel passes to be considered or cumulative passes for both channels to be considered..?

Regards,
Manohar.

 

 

--

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVubkQWFGHa70Wg-rztp22TzE0fmybM=5PWPP0yjm8qEAegA@mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1649153269.S.14357.28649.f5-224-101.1649156519.452%40webmail.rediffmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...