Tuesday, April 5, 2022

Re: [MW:33025] Qualification of Different group Nos for P1 material having Impact & PWHT

Hi,
No. Group Number is a Supplementary essential variable.


Thanks& Regards,

(Karthik)
Karthikeyan.S
M: +66-892512282


On Monday, April 4, 2022, 04:25:20 PM GMT+7, Brijesh Maurya <brijeshmaurya492@gmail.com> wrote:


Dear experts,
I have query regarding QW-403.5
In my job, both impact & Pwht applicable.

My query is, If I qualify PQR with P1G1 with P1G2, then will my WPS be qualified for P1G1 TO P1G2, P1G1 WITH P1G1 & P1G2 TO P1G2?
Welding process: GTAW+SMAW & GTAW ( 2 PQR)



Regards,
Brijesh Maurya

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOBi_ePMA%2BKEJsoZcR3Amts2ZjmTPoQF%2ByWX5_1EEqB44Vwi4g%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...