Thursday, September 30, 2021

Re: [MW:32538] change in sfa number

SFA no is not essential, only Fno & Ano is essential

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Thu, Sep 30, 2021 at 8:51 AM Chaudhary Zafar Iqbal <chzaiqbal88@gmail.com> wrote:
Hello good evening all experts
Can we use E71T1-1C-H4/H8 AWS SFA 5.36 filler wire instead of E71T1-1C-H4/H8 AWS SFA 5.20 if yes then please send me any  reference from code and standard by ASME-2C or SEX 9 or SAES- W12 or W11 or any international standard because our WPS is qualified on AWS 5.20 but we recieved Consumable material AWS SFA 5.36.         This attached label is recieved material 

Regards ,
Zafar 
00966544639978 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP9k9XfupDcLPwdc9kiJyUMxaU%2Bhz%3DHr13PVMmsgj_bO%3Dy_OEw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNvjT6LLE6R8TFyPw1EbZfBY_uS21dhtadb4xDsqtLkDA%40mail.gmail.com.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...