Wednesday, September 29, 2021

Re: [MW:32532] Fabrication of Tanks in the Cold countries with Ambient temperature of -40 deg. C

Please see the requirements for ASME Sec VIII Div-I snap shot on lowest temperature during welding.

Inline image

Please check the particular Design and Fabrication Code and specification for the minimum permissible temperature and take action accordingly.

Thanks & Regards

J.Gerald Jayakumar



On Wednesday, 29 September, 2021, 08:45:53 am IST, N VENKATESWARA PRASAD <weldengr.velosi@gmail.com> wrote:


Dear All,

What are the precautions required to fabricate the Tanks of ASTM A 537 cl1 of thickness varies from 8-20mm with 6 to 10 m height. What are the precautions required.  If any one is having this experience, please provide your contact details.  I will contact you.

Regards

N.V. PRASAD
+968 98511695 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAL%3D4YYiYcaWxTi8TDo_36HzuJaPCTCW_O%3D_W89WoD_W8C_sD-Q%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...