Dear sir,
Please note that qualification for WPS and welder are deference
For welder, he can weld F, H, V but PQR/ WPS must be qulified more
Vào Th 5, 2 thg 9, 2021 lúc 10:37 Vishwas Keskar <vvkeskar123@gmail.com> đã viết:
AWS Table is very clear for WPS PQR.For each position ,PQR is needed .Qualify PQR positions based on envising Production Welding Joint positions.For Welder , range for Qualified position is given based on WPQ tested position.On Wed, 1 Sep 2021, 17:20 DINESH KUMAR DEVENDHIRAN, <dineshqc05@gmail.com> wrote:Dear ExpertsI need a clarification on AWS table 4.1 vs 4.10As per table 4.1- for 3G position WPS shall be qualify for vertical position onlyAs per table 4.10 - for 3G position welder will qualify for Flat, Horizontal, vertical.My doubt is if i have a WPS for 3G uphill position, can i use the same WPS for 1G&2G also ?If not please explain.--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/571704be-652c-417c-9c67-6400ec82034an%40googlegroups.com.
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3P7Fs6c5nxzvj3o8SABXy9ePm0VZdkkxQV2n84iCYgU7Q%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHTP-OmxfT5VF%3D6iDqtp%3DnCvh0_zLLHCTShPQdt8zqK5_7mrgg%40mail.gmail.com.
Comments