Re: [MW:32511] QT stamp on Quenched and Tempered forgings

Check your MTC for the type of Heat Treatment performed and take necessary action with the concurrence of your Client.

Thanks & Regards

J.Gerald Jayakumar



On Tuesday, 7 September, 2021, 10:18:06 am IST, vivek kb <vivekkb87@gmail.com> wrote:


Dear Experts,

Below is an excerpt from ASME SA-350 and is related to product marking:

image.png

Could you please advise the basis of this requirement. In most cases, this stamping is specified for Quenching and tempered or Quenching and precipitation heat treated only unlike the Normalizing or Normalized and tempered.

Regards,
Vivek.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB3WdPMJ0Rz4F0ZaRKJiFx_HkZbr%3DpNiOhtqKiMdEM6AA4%3DSwA%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...