Re: [MW:32510] QT stamp on Quenched and Tempered forgings

Toughness value will be  more than Normalizing, Welding related issues will be more in QT if proper procedure is not followed. 

On Tue, Sep 7, 2021, 10:18 AM vivek kb <vivekkb87@gmail.com> wrote:
Dear Experts,

Below is an excerpt from ASME SA-350 and is related to product marking:



Could you please advise the basis of this requirement. In most cases, this stamping is specified for Quenching and tempered or Quenching and precipitation heat treated only unlike the Normalizing or Normalized and tempered.

Regards,
Vivek.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB3WdPMJ0Rz4F0ZaRKJiFx_HkZbr%3DpNiOhtqKiMdEM6AA4%3DSwA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePHsJS0pYnNu0X6Z%3Dskw17%2B%2BDpCAgUkEXy%2B-srL_e2ZHA%40mail.gmail.com.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...