Dear Expert

Can some help to get the distortion acceptance criteria to WQT at 4G position.

--

--
Best Regards
Samiulla Syed,
Senior Trainer,
Welding Department,
TUV Rheinland Arabia LLC
National Industrial Training Institute,
Al Ahsa,
Eastern Province,
Kingdom of Saudi Arabia,
Email: ssyed@niti.edu.sa
          qcsyedsami@gmail.com
Mobile: +966(0)595531593.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFRNJK8xjqNeVZqH8mPSiJXiGOeyRarkk%3Dj3qytygKrBKVVRMA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...