Check with SHAW DEWPOINT METER.

On Sun, 28 Jun 2020 11:44 am Charles Jacob, <charlesvj@gmail.com> wrote:
Dear , 

In SFA 5.32 which gives the requirements for shielding gases, the requirement is to mention % composition to check if it is a single gas or mixed gas. So the code is not asking about the purity of the gas. 
     Purity of the gas is mentioned seperately as 99.997 %. This is more of a procurement parameter rather than welding.  
    As per my opinion, one should mention the percentage composition of the gas rather than purity in the wps format. 

Regards,

Charles V Jacob.

On Sun, Jun 28, 2020, 7:31 AM 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:
The reason for having purity % in WPS is to check whether you use Single or mixture of gases which is an essential variable. Welding Grade Argon purity as per ASME Sec.IIC is 99.997%. In addition to this for Duplex & SDSS we mention the Oxygen ppm levels in the PQR & WPS

Thanks & Regards

J.Gerald Jayakumar



On Saturday, June 27, 2020, 09:24:03 PM GMT+7, Raja Varman <peraiyur.varman@gmail.com> wrote:


Normally you can get the Test certificate from the gas supplier about the purity of the gas.

Its enough to confirm the purity for WPS requirements.

என்றும் அன்புடன்,
Thanks & Regards,
RAJAVARMAN
+971561895584

On Fri, Jun 26, 2020, 7:35 PM Vinayak <vinayaknaik57@gmail.com> wrote:
what is the instrument name to check purity.

On Saturday, April 5, 2014 at 4:41:41 PM UTC+5:30, Richard robes wrote:
Mr.Prabhu,

You can check with Argon gas meter / Analyzer for 99.9 % purity or as per WPS requirements. Hope it's clear.

Regards
Richard


On Fri, Apr 4, 2014 at 4:18 PM, Maulik Thakkar <mlkth...@gmail.com> wrote:

You want to check which impurity?

Normally moisture/dew point need to be checked as per AWS 5.32. It should be less then 10.5 ppm.

To check moisture, dew point analyzer is available.

Regards,
Maulik
L&T, Welding engg. & Metallurgy

On Apr 4, 2014 5:31 PM, "prabhu" <prabhuj...@gmail.com> wrote:
Dear All,
 
I my doing work on SS material 316L , ensurinig clean and dust free area and surface but enable to rnsure the Argon gas purity.
please guid me how to ensure the gas .
Or is there any divice to check the Argon gas impurities.

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to material...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to material...@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to material...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to material...@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2b2c6a22-9f2c-4984-957c-4b0cebb443a0o%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BHpzU7bqMTz3ZRs7_2uZc98yoAbwmzT%3DysS0LAf%2BqhNvY_WnA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2119216742.3318610.1593295493805%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKpzM4BTvNiu6Dx41bPoCL72xSqKt4o87YZo069jTWkfK%3D_-DA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOhdV_crVk7S_hfbKSYWqd_x64B7vtb4F--Qqsc2aDAtQ%40mail.gmail.com.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...