Tuesday, June 16, 2020

Re: [MW:31009] HIC requirement in SS316

Pls go through nace tm0284

Sent from my iPhone

On 16-Jun-2020, at 8:58 AM, Vivek Mane <vivek12787@gmail.com> wrote:


Dear Experts,

Kindly share your views on whether the HIC test is done on SS 316 material.
If yes then for which temperature/service it is done. Also give reference to any code/reference.
Thank you in advance.

Regards,
Vivek V.Mane
BVIL Mumbai
08693002244

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAK4-NK81SzbxxvYiB0CSRAs1nN75VE8FfOOHL-Y%3D5g3MyCdqAg%40mail.gmail.com.

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon

Hi As its %elongation is very low  Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...