Monday, June 15, 2020

Re: [MW:31005] Filler rod selection for SS 304L to SA 335 pipe welding

Hi,
For high temperature service, ER312 or E312 is not a good choice due to difference in coefficient of thermal expansion between 312 and ferritic steel which cause early failure.

On Monday, 15 June 2020, 04:39:14 GMT+1, harenath jha <harenathjha@gmail.com> wrote:


Basis of selection please ?

On Sun, Jun 14, 2020, 21:39 Chintan <chintan51@gmail.com> wrote:
Use ER312 & E312

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b498dd65-4ebe-4eca-827a-7db9e5f691a5o%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPRS9UOr8MuMLc_AW3a6tKqZBJsc_O6XYbz4i6vDHLC5AD-kow%40mail.gmail.com.

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon

Hi As its %elongation is very low  Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...