Monday, June 15, 2020

Re: [MW:31003] Filler rod selection for SS 304L to SA 335 pipe welding

Basis of selection please ?

On Sun, Jun 14, 2020, 21:39 Chintan <chintan51@gmail.com> wrote:
Use ER312 & E312

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b498dd65-4ebe-4eca-827a-7db9e5f691a5o%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPRS9UOr8MuMLc_AW3a6tKqZBJsc_O6XYbz4i6vDHLC5AD-kow%40mail.gmail.com.

No comments:

[MW:35633] IP Joint